Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27

Cover of: Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27 |

Published by National Aeronautics and Space Administration, Scientific and Technical Information Branch, For sale by the National Technical Information Service,] in [Washington, D.C.], [Springfield, Va .

Written in English

Read online

Subjects:

  • Aluminum-chromium alloys.,
  • Iron-nickel alloys -- Mechanical properties.,
  • Iron-nickel alloys -- Oxidation.,
  • Aluminum.,
  • Chromium.,
  • Iron alloys.,
  • Mechanical properties.,
  • Oxidation.,
  • Tensile strength.

Edition Notes

Book details

StatementSusan R. Schuon.
SeriesNASA technical paper -- 2443.
ContributionsUnited States. National Aeronautics and Space Administration. Scientific and Technical Information Branch.
The Physical Object
FormatMicroform
Pagination1 v.
ID Numbers
Open LibraryOL16114913M

Download Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27

25787 views Monday, November 30, 2020